POM copolymer Product with reduced emissions especially for automotive interior application. Good properties of the standard-injection molding grades like high rigidity, hardness and toughness; good chemical resistance to solvents, fuel and strong alkalis as well as good hydrolysis resistance; high resistance to thermal and oxidative degradation are maintained Burning rate ISO 3795 and FMVSS 302 < 75 mm/min for a thickness more than 1 mm. VDA 275 Emissions < 10 ppm Ranges of applications: automotive engineering, FMVSS = Federal Motor Vehicle Safety Standard (USA)
| Yoğunluk (g/cm³) | 1.41 |
| Akış Hızı (g/10 min) | - |
| Alev /Yanıcılık Derecesi | - |
| Çentikli Izod Darbesi ASTM 256 (J/m) | - |
| Çentikli Izod Darbesi ISO 180 (kJ/m²) | - |
Bu ürün için hiçbir özellik listelenmemiştir.