POM copolymer Standard Injection molding type, UV-stabilized with UV-stabilizers.; good chemical resistance to solvents, fuel and strong alkalis as well as good hydrolysis resistance; high resistance to thermal and oxidative degradation. Burning rate ISO 3795 and FMVSS 302 < 100 mm/min for a thickness more than 1 mm. FMVSS = Federal Motor Vehicle Safety Standard (USA)
| Densità (g/cm³) | 1.41 |
| Fluidità (g/10 min) | - |
| Fiammabilità | - |
| Prova di impatto Izod ASTM 256 (J/m) | - |
| Prova di impatto Izod ISO 180 (kJ/m²) | - |
Non ci sono specifiche per questo prodotto